Fasaloli na Fasaha na Fangding Glass Lamination Firewall

1. Jikin murhun yana amfani da tsarin ƙarfe, kuma murhun yana amfani da haɗin kayan kariya na zafi guda biyu na kayan kariya na zafi masu inganci da sabbin kayan kariya na zafi. Ƙara yawan zafin jiki cikin sauri, ingantaccen tasirin kariya na zafi, ƙarancin asarar zafi da adana kuzari.
2. Tsarin sarrafa zafin jiki mai wayo wanda aka haɓaka da kansa, dukkan tsarin yana gudana ta atomatik, kuma yana farawa da maɓalli ɗaya. Tare da ƙararrawar kuskure, aikin nazarin kurakurai, aikin ƙararrawa ta atomatik bayan aiki, babu buƙatar ma'aikata su yi tsaro.
3. Ana iya daidaita wutar dumama ta atomatik, dumama tana da sauri kuma yawan amfani da makamashi ya ƙanƙanta
4. Ana iya daidaita matsin lamba na injin ta atomatik. A lokacin narkewar fim ɗin, ana iya guje wa abin da ya faru na cikar manne na fim mai kauri saboda matsin lamba mai yawa.
5. Yana da aikin kashe wuta da kuma kula da matsin lamba. Bayan an kashe famfon injin, jakar injin zata iya kula da injin ta atomatik ba tare da kariya daga ma'aikata ba. Bayan an kunna wutar, zai iya ci gaba da aiki don hana faruwar gilashin da aka yi wa shara laminate.
6. An yi jakar injin tsabtace gida da farantin silicone mai jure wa hawaye, wanda yake da ɗorewa kuma yana da iska mai kyau.
7. Bututun dumama yana amfani da bututun dumama bakin ƙarfe na nickel, wanda ake dumama shi daidai gwargwado da kafet kuma yana da tsawon rai. Fanka mai zagayawa zai iya sa saman sama da ƙasa na kowane Layer na jakunkunan tsotsa ya yi zafi daidai gwargwado.
Matakan samar da gilashin laminated:

1. Bayan an haɗa gilashin da aka tsaftace da fim ɗin EVA da aka yanke, sai a saka shi a cikin jakar silicone. Ana iya tara gilashin da aka laminated ɗaya bayan ɗaya. Domin hana ƙaramin gilashin motsi, ana iya gyara gilashin da tef mai jure zafi a kusa da shi. Yana da kyau.
2. Yana da kyau a sanya mayafin a kusa da gilashin don fitar da hayaki mai amfani da iska, sannan a sanya famfon sanyi na tsawon mintuna 5-15 a zafin ɗaki don zubar da iskar da ke cikin jakar silicone.
3. Gabaɗaya, zafin saman gilashin ya kai 50°C-60°C, kuma lokacin riƙewa shine mintuna 20-30; sannan a ci gaba da zafi har sai zafin saman gilashin ya kai 130°C-135°C, kuma lokacin riƙewa shine mintuna 45-60. Kauri na fim ɗin ko adadin yadudduka masu laminated yana ƙaruwa, ana iya tsawaita lokacin riƙewa yadda ya kamata.
4. A lokacin sanyaya, ana buƙatar a kula da injin tsabtace iska, kuma ana iya amfani da fanka don sanyaya iska.
Lokacin Saƙo: Yuli-08-2022